Author: Holland RI

Source: European Journal of Oral Sciences.

Year: 1984

Comment:

Abstract / Excerpt:

Galvanic corrosion of amalgam, induced by contact with a type IV dental casting gold alloy, was determined under simulated oral conditions in an electrochemical cell. The effect of a pellicle layer formed by 1 h exposure to saliva in the oral cavity was determined. Pellicle on the amalgam had no effect on the maximum corrosion rate or the 2 h corrosion charge, whereas pellicle on the gold alloy substantially reduced both these parameters of the conventional low-copper amalgam; the corrosion of the high-copper amalgam was less and was not influenced by pellicle formation.

Citation: HOLLAND RI. Effect of pellicle on galvanic corrosion of amalgam. European Journal of Oral Sciences. 1984;92(1):93-6.